Week 1 · Lesson 1.4
Growing crystals and slicing wafers
From pure chunks to a perfect crystal to slices thinner than a fingernail.
Pulling a perfect crystal
Polysilicon is melted at about 1,420 °C with a tiny pinch of (gallium or boron).
In the method, a seed crystal touches the melt and is pulled up slowly while turning. Atoms line up behind it, making a about 2 m long.
Pull too fast and the crystal breaks its pattern, the ingot is downgraded.

1 of 6